I'm trying to make carbon tube by hand layup process. after wetting and wrapping the fabric around the mandrel i wrap peelply, perforated film and breather around it and vacuum it but after curing, the carbon fabric is wrinkled in several places. i didn't use a vacuum gauge but it did seem there was a leakage . what could be the reasons? what can i do to avoid this?