For a component size of 400 square cm is a 3 CFM apt?
oekmont
oekmont
Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
Theoretically you could infuse giant structures with a small pump. It's mainly convenience to use bigger pumps for bigger parts. 400cm^2 is quite small anyways, so you could use a pump of any capacity.

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search