As long as the detail is not too deep then the resin will fill it no problem as it is quite runny.
With matt finishes, be aware your silicone mould will mechanically grip the part slightly so may need peeling off a bit more carefully and may have a reduced lifespan. You can mitigate against this a little by rubbing some pure silicone oil onto the mould or using a silicone release spray.