Easy Composites Ltd Technical Support
»
Easy Composites Ltd - Product Specific Pages
»
Resins, Gelcoats and Pigments
»
Cheaper Resin Equivalent - XTC-3D
Cheaper Resin Equivalent - XTC-3D
Post Reply
Like
8
Cheaper Resin Equivalent - XTC-3D
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
David Nicholls
David Nicholls
posted 6 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 4
Hi
I currently use this product to coat FDM 3d prints prior to finishing/painting.
https://www.smooth-on.com/product-line/xtc-3d/
XTC-3D
Have you got a resin in your range that has similar properties but is more cost effective? I think it mainly the "slump" that I'm trying to retard slightly so the resin stays on vertical surfaces whilst setting.
Ideally I'd like it clear or with minimal colour for self coloured prints.
Regards
Dave Nicholls
Reply
Like
8
Reply
Warren (Staff)
Warren (Staff)
posted 6 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
Fumed silica
will add to the thickness of the resin although add only very small amounts (less than 1%) as it can make the resin very thixotropic if you put in too much.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Cheaper Resin Equivalent - XTC-3D
David Nicholls
-
6 Years Ago
Couldn't see any pricing on there to compare with, however it seems a similar product to our XCR Epoxy Coating Resin which is commonly used for similar applications on 3D prints and other patterns.
Warren (Staff)
-
6 Years Ago
Hi - I'd guess you're at about 70% of the XTC-3D price. I purchased a small kit of XCR Epoxy Coating Resin and coated some test pieces. Still getting some print layer lines showing through though......
David Nicholls
-
6 Years Ago
Fumed silica will add to the thickness of the resin although add only very small amounts (less than 1%) as it can make the resin very thixotropic if you put in too much.
Warren (Staff)
-
6 Years Ago
Post Reply
Like
8
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search