I saw many videos about how to using 2 mould to create stuff, usually lay composite on each mould separately, while the problem is when people are doing this, the joint place got no composite connected, they are only glued together, how to strength that part I am wondering, I guess this is a very common questions most people will encounter. Let's discuss it a little bit, how to solve it? if not possible or too hard, how to bypass it? Thanks.
Reply
westcomposite
w
Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)
Group: Forum Members
Posts: 11, Visits: 43
Thanks, Scott.

I am looking to do a bent pipe with manifold. I guess the best way is to split to two, however, feel it is hard keep the shape inside and strength at the joint place.

Actually, I want the inside surface of pipe to be smooth too, if I put a mould inside, how can I remove the inside mould? If I don't have a inside mould,  how can I be sure the 10mm margin stick to the other side, using finger or any tool to stroke is not precise. So, actually, many questions here. Don't have a clue.