Dennis G
Dennis G
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 34,
Visits: 837
Quick question about the connectors. I want to make sure I buy the right stuff. The picture of the connectors show slots on 4 sides of the connector. When I watch the
How to do Perfect Resin Infusion for Cosmetic Carbon Fibre Parts
it shows one connector has a straight across slot for the Spiral and the other connector has three slots for the vacuum pump side.
So my question is.....when you purchase the
Resin Infusion Silicone Connector from the web site what do you get? Do you get the pair described above or do you just get one 4 way connector? Did the connectors in the video get replaced? I just want to order the correct stuff.
Thanks,
Reply
Like
9
Reply
Hanaldo
Hanaldo
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Thanks Aj, pretty much along the lines of what I was thinking, though the way you worded it has made up my mind on how to do it. Funny how bouncing ideas around can eliminate indecisiveness
Reply
Like
8
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Resin infusion silicone connectors
Dennis G
-
13 Years Ago
I received the ones with 4 slots. It doesn't matter, these work the same way as long as there is...
NikCFC
-
13 Years Ago
The design of the silicone connector has been improved with both a change to the 4 slot design you...
Warren
-
13 Years Ago
Hi Warren, Good point, I've just put something on the product page now. We intend to show the...
Matt (Staff)
-
13 Years Ago
Another question about these connectors. How long are they sopose to last? It seems the more I use...
Dennis G
-
12 Years Ago
The connectors will work until they break up. The connector should still be flexible enough to break...
Warren (Staff)
-
12 Years Ago
Bit of a thread revival, but I just wanted to ask how these silicone connectors are made? I...
Hanaldo
-
11 Years Ago
I imagine they will just be cast silicone in a mould judging by the flash you get on new ones. Would...
ajb100
-
11 Years Ago
Thanks Aj, pretty much along the lines of what I was thinking, though the way you worded it has made...
Hanaldo
-
11 Years Ago
Post Reply
Like
9
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search