Group: Forum Members
Posts: 6,
Visits: 38
|
Hi, I am in the process of making a mould that I want to use with prepregs to make a brake lever, so far I have taken a mould of the lever using the easy composites epoxy mould starter kit (green gel coat). I want to make a pattern from this mould and then a final mould from that, that can be used with prepregs in an oven. My question is what should I use to make the pattern? My understanding is that it will need to cure at a low temperature but then be post cured to a much higher temperature in order to make a final mould from it using tooling prepreg? Sorry if my terms are incorrect, this is all new to me. Thanks, Luke.
|