vaccum bagging dramas


Author
Message
igs_au
i
Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)
Group: Forum Members
Posts: 9, Visits: 67
Hi all, I'm making a carbon fiber part with a basic bend, no dramas there. All parts sorted. I've got a vacuum pump, basic oil based. It creates vacuum alright, but when I switch it off, air comes back into the bag and no more vacuum. It's a bit frustrating really. Should I just keep the pump running until the whole thing at least starts to cure? I've got the bag sealed ok, I think, and the connector, which I made myself, looks solid. When the pump is running, you can see that the pipe is flattened, sucking all air out. and when I switch the pump off, the pipe fills with air again. Very frustrating. Any advice would be great.

Replies
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
igs_au - 5/22/2019 10:54:20 PM
Hi all, I'm making a carbon fiber part with a basic bend, no dramas there. All parts sorted. I've got a vacuum pump, basic oil based. It creates vacuum alright, but when I switch it off, air comes back into the bag and no more vacuum. It's a bit frustrating really. Should I just keep the pump running until the whole thing at least starts to cure? I've got the bag sealed ok, I think, and the connector, which I made myself, looks solid. When the pump is running, you can see that the pipe is flattened, sucking all air out. and when I switch the pump off, the pipe fills with air again. Very frustrating. Any advice would be great.

Some pumps will run backwards when switched off so that lets go of the vacuum.

I think most people leave the pumps running, I do. I also have a one way valve at the pump so it can not run backwards either.





igs_au
i
Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)
Group: Forum Members
Posts: 9, Visits: 67
Fasta - 5/23/2019 1:06:04 AM
igs_au - 5/22/2019 10:54:20 PM
Hi all, I'm making a carbon fiber part with a basic bend, no dramas there. All parts sorted. I've got a vacuum pump, basic oil based. It creates vacuum alright, but when I switch it off, air comes back into the bag and no more vacuum. It's a bit frustrating really. Should I just keep the pump running until the whole thing at least starts to cure? I've got the bag sealed ok, I think, and the connector, which I made myself, looks solid. When the pump is running, you can see that the pipe is flattened, sucking all air out. and when I switch the pump off, the pipe fills with air again. Very frustrating. Any advice would be great.

Some pumps will run backwards when switched off so that lets go of the vacuum.

I think most people leave the pumps running, I do. I also have a one way valve at the pump so it can not run backwards either.


ah thank you. I thought so, Is there a place I can get a valve like that? I did order a cut off valve at the EC today. See how that goes