Hi guy's,

Did a hand layup on my part following the guide, but after sanding the resin back before final lacquer, it seems there was a low spot where I've hit the material and taken a chunk out of the part, see images below.

Any ideas what's best to repair this? Or is it a case if start again?
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
this looks more like you had a bit of a void in the part or bridging and have just sanded out the bubble, I would mix up some resin again and apply to the local area.
Let it cure  and then sand back.


C4RBON94
C
Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)
Group: Forum Members
Posts: 9, Visits: 25
scottracing - 5/19/2019 8:01:30 PM
this looks more like you had a bit of a void in the part or bridging and have just sanded out the bubble, I would mix up some resin again and apply to the local area.
Let it cure  and then sand back.


Ok so is there a way to replace the missing bits of weave or is that a no go?

Lester Populaire
L
Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
C4RBON94 - 5/19/2019 8:11:19 PM
scottracing - 5/19/2019 8:01:30 PM
this looks more like you had a bit of a void in the part or bridging and have just sanded out the bubble, I would mix up some resin again and apply to the local area.
Let it cure  and then sand back.


Ok so is there a way to replace the missing bits of weave or is that a no go?

yeah looks like you had a void underneath and sanded trough the carbon. your best bet would probably be to laminate a patch on top of it which will be structurally sound, but visible. for a cosmetic part you can maybe increase the size of the patch and have the cut line on a ledge, where it's way less visible.

C4RBON94
C
Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)
Group: Forum Members
Posts: 9, Visits: 25
Lester Populaire - 5/20/2019 7:20:17 AM
C4RBON94 - 5/19/2019 8:11:19 PM
scottracing - 5/19/2019 8:01:30 PM
this looks more like you had a bit of a void in the part or bridging and have just sanded out the bubble, I would mix up some resin again and apply to the local area.
Let it cure  and then sand back.


Ok so is there a way to replace the missing bits of weave or is that a no go?

yeah looks like you had a void underneath and sanded trough the carbon. your best bet would probably be to laminate a patch on top of it which will be structurally sound, but visible. for a cosmetic part you can maybe increase the size of the patch and have the cut line on a ledge, where it's way less visible.

Ok, it's quite a large part with minimal edges so I'm not sure if there's a clean way to join it as I'm guessing any join lines would show?

Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yeh if it has to be invisible then its a start again job. If it isn't an extremely obvious area then I would just neatly laminate a patch over the top and live with some visible lines.
Lester Populaire
L
Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
C4RBON94 - 5/20/2019 7:55:16 AM
Lester Populaire - 5/20/2019 7:20:17 AM
C4RBON94 - 5/19/2019 8:11:19 PM
scottracing - 5/19/2019 8:01:30 PM
this looks more like you had a bit of a void in the part or bridging and have just sanded out the bubble, I would mix up some resin again and apply to the local area.
Let it cure  and then sand back.


Ok so is there a way to replace the missing bits of weave or is that a no go?

yeah looks like you had a void underneath and sanded trough the carbon. your best bet would probably be to laminate a patch on top of it which will be structurally sound, but visible. for a cosmetic part you can maybe increase the size of the patch and have the cut line on a ledge, where it's way less visible.

Ok, it's quite a large part with minimal edges so I'm not sure if there's a clean way to join it as I'm guessing any join lines would show?

When you put a patch on top try to align the weave which will help to somewhat reduce the visibility...

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search