Are any casting resins food safe so they can be as inlays on cutting boards?
Reply
Tom (Staff)
T
Supreme Being (201 reputation)Supreme Being (201 reputation)Supreme Being (201 reputation)Supreme Being (201 reputation)Supreme Being (201 reputation)Supreme Being (201 reputation)Supreme Being (201 reputation)Supreme Being (201 reputation)Supreme Being (201 reputation)
Group: Moderators
Posts: 21, Visits: 977
Mark Cooper - 5/16/2019 10:04:18 AM
Are any casting resins food safe so they can be as inlays on cutting boards?

Good Afternoon,
Thank you for your enquiry. Whilst fully cured resin is completely inert, none of the GlassCast range is certified as food safe and so is not recommended where such certification is required. Art Resin is a food safe resin but cures quite soft and will probably not be suitable for things like chopping boards.

If there is anything else i can help you with, please let me know.

Kind Regards

Tom
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search