Hi all,

I'm in the process of getting ready to pour a cylindrical tube out of epoxy or polyester resin. It is 0.5" thick walls with an ID of 14". The cast will be 30" tall and needs with withstand internal pressures of 45psi.

I have obtained metal duct work for the mold sides and an environmental chamber to cast the piece in. I'm looking for any advice on how to apporach casting something of this size (~3gal). Would I have to pour in layers or would it be possible to pour all at once? What sort of resin would be recommended for such a task?

Thank you,

Jon
Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
oekmont - 4/11/2019 9:06:17 PM
Epoxy is by no means a similar material to polycarbonate. That would habe been a descent choice for your application.
If you really want to cast it, and it has to be clear transparent, I guess epoxy (with a slow hardener) would be your "best" option. Polyester usually has even greater problems with internal stress from curing. And everything else won't be transparent. Again, I consider it highly dangerous and would absolutely not try it myself.

Like above, I don't think it is a safe thing to do. epoxy would be your best choice. pouring this in a transparant clear way without bubbles will be extremely difficult with resins. Have you thought on how you will even demould the inner tube? Resin will tend to shrink and make it pretty hard to remove the inner tube without breaking it. have you thought of the post-cure of your epoxy as well? 
I'm a big believer in trying things that haven't been done before but keep it safe. epoxy is strong when used with a matrix but very brittle as well and shatters in sharp shrapnel like glass. theoretical an practical approach in strength are in many times far off. small bubbles or curing cracks will weaken the epoxy a lot compared to labo-tests in best conditions where manufacturers aim for the highest results for their products.  Like in the comments above, comparing it with making a grenade is a good comparison BigGrin 


Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Jonathan Cappola - 6 Years Ago
SleepingAwake - 6 Years Ago
Jonathan Cappola - 6 Years Ago
SleepingAwake - 6 Years Ago
Jonathan Cappola - 6 Years Ago
Jonathan Cappola - 6 Years Ago
oekmont - 6 Years Ago
Jonathan Cappola - 6 Years Ago
oekmont - 6 Years Ago
matthieutje65 - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search