+x Warren (Staff) - 4/4/2019 9:51:02 AMGenerally GlassCast 3 is ideal for counter tops and work tops. GlassCast 3 settles flat as it self levels giving a smoother surface than other clear resins.
+x Einar Valmundsson - 3/10/2020 6:27:29 PM+x Warren (Staff) - 4/4/2019 9:51:02 AMGenerally GlassCast 3 is ideal for counter tops and work tops. GlassCast 3 settles flat as it self levels giving a smoother surface than other clear resins.HelloI´m going to make a Epoxy countertop with mixed colors.My plan is to cote a plate made out of MDFThe look should be Cement grey with some veins.So my questions are:1- Do I need a primer? If so what material would you recoment2- Then I just mix the resin (GlassCast 3) with hardener and coloring pigment.By adding small amount of color I get weak color, If I put a lot I get strong color.3- If I´m happy with the pattern I let it harden4- Then I put GlassCast 3 resin layer over the color.