How much heavier is a product made with resin infusion compared to prepreg?


How much heavier is a product made with resin infusion compared to prepreg?
Author
Message
John Hansen
J
Supreme Being (379 reputation)Supreme Being (379 reputation)Supreme Being (379 reputation)Supreme Being (379 reputation)Supreme Being (379 reputation)Supreme Being (379 reputation)Supreme Being (379 reputation)Supreme Being (379 reputation)Supreme Being (379 reputation)
Group: Forum Members
Posts: 42, Visits: 232
In another thread I asked about resin uptake of Balsa when used as a core. I have received various answer that are not answering the question, so let me go at it a different way.

If identical composite parts are made using any available method such as - but not limited to - hand layup, resin infusion, or prepreg, with a core of unsealed balsa and sealed balsa, Which would be the lightest and by how much would the weight difference be?

On another forum, I have received replies that seem to presume that it is common knowledge that resin infusion will weight a LOT MORE than if the parts are made with prepreg. Maybe all the old timers know this to be true and never use resin infusion to make light balsa core products.

But really now.... How much more is a LOT MORE?

Is there any data that will tell me how much heavier one is compared to the other?

For this discussion, please do not confuse the question by bringing up other core materials that you might think are better, lighter, stronger. That discussion will be a separate topic. First I want to know about balsa core.


A Lifelong Learner

Edited 6 Years Ago by John Hansen
Replies
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
When talking about infusing only a solid laminate it is likely you can get an equal resin content to pre pregs.

As mentioned above though when you add in any cores, with their edges, open surface cells of foams, bridging from a vac bag then all these gaps will fill with resin too and can make for heavier parts.

I have built the same small boat design in both pre pregs and infusion. The infused hull was exactly 10% heavier. Pre preg = 10kg , Infused = 11kg. The laminates will still have a great resin/fibre ratio but all the gaps will be full of resin. With balsa there maybe a chance that you infuse the wood too. Super strong but heavy.

Balsa is cheap, that's why they use it !






Edited 6 Years Ago by Fasta
John Hansen
J
Supreme Being (379 reputation)Supreme Being (379 reputation)Supreme Being (379 reputation)Supreme Being (379 reputation)Supreme Being (379 reputation)Supreme Being (379 reputation)Supreme Being (379 reputation)Supreme Being (379 reputation)Supreme Being (379 reputation)
Group: Forum Members
Posts: 42, Visits: 232
Fasta - 3/26/2019 7:50:39 AM
When talking about infusing only a solid laminate it is likely you can get an equal resin content to pre pregs.

As mentioned above though when you add in any cores, with their edges, open surface cells of foams, bridging from a vac bag then all these gaps will fill with resin too and can make for heavier parts.

I have built the same small boat design in both pre pregs and infusion. The infused hull was exactly 10% heavier. Pre preg = 10kg , Infused = 11kg. The laminates will still have a great resin/fibre ratio but all the gaps will be full of resin. With balsa there maybe a chance that you infuse the wood too. Super strong but heavy.

Balsa is cheap, that's why they use it !



Thank you Fasta. This is very valuable information. If 10% is an attainable figure for my project which is a UAV frame/hull, it will round out to about 100 to 150 gram difference. So, all things being equal, the powerplant and battery system will need to lift that extra weight 100% of the time. It does not seem to be enough of a difference to not consider using infusion. This encourages me to move forward.


A Lifelong Learner

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
HansenJC - 6 Years Ago
Warren (Staff) - 6 Years Ago
HansenJC - 6 Years Ago
matthieutje65 - 6 Years Ago
oekmont - 6 Years Ago
Fasta - 6 Years Ago
HansenJC - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search