If you are pulling down a large bag or against a leaky bag, sometimes you can exceed the separator's capacity to filter. In essence it drains down through a small hole in the bottom and once full of oil it needs a minute or so to drain down. Under typical load or once under a full vacuum you should not notice any issues with the separator.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|