Group: Forum Members
Posts: 550,
Visits: 27K
|
Do you have photos from different angles? To me it looks like you could do it in a two piece mould, if you "cut off" the outer recess on the left side with the second mould piece and demould the main piece to the right. I would definitely advice not to use silicone mould pieces in the way you intend to do. You will get bad surfaces at the junction between the materials, and the cicles for the lamps will definitively not end up perfectly round.
|