Well here is another one, should have been the first question? Lol

Having discussions with friends, not being aware what's up my sleeve...they are concerned with yellowing of CF due to exposure to the sun/water etc... I read about your gel coats:

 Gel coats are generally applied as a thickness of 0.3-0.7mm and are specially formulated to provide the part or mold surface with properties such as resistance to UV (ultraviolet) degradation, hydrolysis or osmosis (where water is absorbed into a composite over considerable time)

As mentioned on your site your products are superior to other products on the market...could elaborate on it some?


What thickness would give the best result? .7mm?
How would I measure the thickness? would it be in terms of coats, before CF layied?


When I plan to make the heat shield for my bike I will use the

Clear Epoxy Gel Coat correct?

Should have asked this question in the 1st post my bad......
Reply
Carbon Tuner
Carbon Tuner
Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)
Group: Forum Members
Posts: 104, Visits: 422


hmmmmmmmm,I like that!



Soyour infusion resin is compatible, but where can I get the lacquer? Would asimple airbrush system work to apply it to the mold? how thick is the rightamount?





If Brute Force Isn''''t working your not using enough...
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search