The problem you have is most resins and adhesives are not designed for that temperature range when it comes to curing. The cure times can be significantly extended and even stalled completely if cold enough. We do not have anything specifically designed for curing at lower temperatures.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|