The absolute best thing you can do both for your confidence and your end result; is buy a little bit extra resin and play around with it a bit first. Do a couple of small jobs with 200g of resin and see how the resin works, how it feels, how thick and hard it is to mix, how its going to behave in your specific work environment. It blows my mind how many people with little to no prior experience with epoxy resin of any sort buy 25kg of resin, mix it all up and tip it on their floor and then panic when things go wrong.
At the end of the day, you just have to respect the chemistry at play. These are excellent products, and they are very user friendly, but they are still a chemical and can be unforgiving if the instructions are not followed meticulously. Pay attention to the ambient temperature in your work environment, if it is below 20° dont be impatient and go for it anyway, make sure it is above 20°. Work clean, spend the time cleaning your floor and your mixing area to make sure no contaminants can ruin your result. Be very accurate with your mix ratios, and spend plenty of time mixing, dont rush the mixing process. Dont try to mix huge batches, it's much easier to mix 1kg at a time and do several pours than it is to mix 5kg. With epoxy, it is extremely rare indeed that anything will go wrong if the working temperature is correct, the mix ratios are bang on, and the two components are thoroughly mixed.
|