Hello everyone,

I'm new in the forum, and already have my first question :-)

Who is able to do me a non-binding rough breaking-strength calculation for following sailing-boat-part made of carbon? Example pic at the end of this text.

It is about a so-called BOWSPRIT pipe (for the gennaker sails).

I'd like to change my old aluminum one for a carbon one.

My old aluminum tube has 8.5kg incl all fittings. The carbon tube only 2.5kg.
I haven't used it yet. I would like to ask forum experts first.

Conclusio should be: Is the carbon tube sufficiently dimensioned or at least as stable as the one made out of aluminium?

I have following info for you:

old aluminium tube:
- alloy: probably AlMgSi0,5
- Length: 2,300mm (approx. 1 meter boom, the rest is screwed on deck with 2 clamps)
- outer diameter: 80mm
- Inside diameter: 72mm
- Wall thickness thus: 4mm
- Weight of the pipe without fittings approx. 8 kg

Carbon tube:
pullwinded
- Length: 2,300mm (approx. 1 meter boom, the rest is screwed on deck with 2 clamps)
- outer diameter: 80mm
- Inside diameter: 76mm
- Wall thickness thus: 2mm

fiber alignment: Unidirectional inside + 75°/35° outside
fiber volume: aprox. 60 %
surface: smooth, shiny
temperature resistance: up to 110 °C
tensile-E-Modul: 240.000 MPa
tensile strength: 4.000 MPa
fracture strain: 1,50%
density: 1,8/cm³
thermal expansion coefficient: -0,1 * 10-6*K-1 along the fiber
radiolucent: 100%
specific elctrical resistance: 1,6*10-3Ohm*cm
heat conductivity: 17 [W/(m*K)]
specific heat capacity: 710 [J/kg*K)]
no vibrations
UV-resistent by using standard varnish
corrosion-resistent: e.g. petrol, oil, saltwater, hydrofluoric acid
handling: drill, mill, cutt, glue 

weight: approx. 1kg per meter

Would be super nice of you if you could help me

Many thanks in advance




BR
Carbon-Charly

Edited 6 Years Ago by Carbon Charly
Reply
Carbon Charly
Carbon Charly
Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)
Group: Forum Members
Posts: 7, Visits: 86
Hi Oekmont.
This was very very kind of you. Thank you very much for your help !
The company who sold me the tube is just seller and not manufacturer. I will ask them that they schould ask their supplier to get more info about the tube. Which parameters would be the most important ones to make a detail calculation?
br

P.s. Oek + Mont = Leoben ?


BR
Carbon-Charly

Edited 6 Years Ago by Carbon Charly
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
carbon-charly - 6 Years Ago
oekmont - 6 Years Ago
carbon-charly - 6 Years Ago
carbon-charly - 6 Years Ago
oekmont - 6 Years Ago
carbon-charly - 6 Years Ago
oekmont - 6 Years Ago
carbon-charly - 6 Years Ago
oekmont - 6 Years Ago
Zorbit - 6 Years Ago
Zorbit - 6 Years Ago
carbon-charly - 6 Years Ago
oekmont - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search