+x f1rob - 12/25/2018 12:05:18 PMTo be fair not that much more.Put a vernier on a piece of uncurred umaterial an that's the thickness you will get cured,be it 15psi or 90 Just loose a little bit on a ply stack with multiple layers as one layer fits into anotherDon't really need 90psi,but your 100% it's in the cornersEven 30psi will give you 99% success