Hi everybody,

does somebody know where to get stud bonding fasteners in Germany? I need 5 pieces of this:

Stainless Steel Threaded Stud Bonding Fasteners - 19mm Round - M5 x 16mm

I found a shop where you can order it in UK, but only 100pcs a time - that would mean paying about 90 Pound which is a bit to much.
I am also open for alternative ideas Wink

Thanks

Steve Broad
Steve Broad
Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
SHaas - 12/19/2018 4:52:57 PM
Hi everybody,

does somebody know where to get stud bonding fasteners in Germany? I need 5 pieces of this:

Stainless Steel Threaded Stud Bonding Fasteners - 19mm Round - M5 x 16mm

I found a shop where you can order it in UK, but only 100pcs a time - that would mean paying about 90 Pound which is a bit to much.
I am also open for alternative ideas Wink

Thanks

https://www.bighead.co.uk/the-original-bighead/

https://www.hall-fast.com/fasteners-small-components/bighead-bonding-fasteners/bighead-male-threaded-studs
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Easy Composites stock BigHead fasteners. Not sure if they have M5x16, but probably.
SHaas
S
Supreme Being (607 reputation)Supreme Being (607 reputation)Supreme Being (607 reputation)Supreme Being (607 reputation)Supreme Being (607 reputation)Supreme Being (607 reputation)Supreme Being (607 reputation)Supreme Being (607 reputation)Supreme Being (607 reputation)
Group: Forum Members
Posts: 46, Visits: 384
Hanaldo - 12/20/2018 12:18:02 PM
Easy Composites stock BigHead fasteners. Not sure if they have M5x16, but probably.


No they do not have them. And the best would be a provider in Germany because it is not that nice to pay more for Fedex than for the studs Smile

Steve Broad
Steve Broad
Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
SHaas - 12/20/2018 12:22:40 PM
Hanaldo - 12/20/2018 12:18:02 PM
Easy Composites stock BigHead fasteners. Not sure if they have M5x16, but probably.


No they do not have them. And the best would be a provider in Germany because it is not that nice to pay more for Fedex than for the studs Smile


https://shop.kvt-fastening.de/en/itemgroup/2001.html
Steve Broad
Steve Broad
Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
Hanaldo - 12/20/2018 12:18:02 PM
Easy Composites stock BigHead fasteners. Not sure if they have M5x16, but probably.

They only go down to M6 and charge £1.86 each!

Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Fair enough, I hadn't checked the sizes. I tend to only use M6 and M10. 

And £1.86 each isnt THAT bad for small quantities!
Steve Broad
Steve Broad
Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
Hanaldo - 12/20/2018 10:45:37 PM
Fair enough, I hadn't checked the sizes. I tend to only use M6 and M10. 

And £1.86 each isnt THAT bad for small quantities!

I think that their prices have dropped so, I agree, that this isn't too bad for small numbers. However, I tend to buy in bulk and paid just under a £1 each for mine (similar size).

SHaas
S
Supreme Being (607 reputation)Supreme Being (607 reputation)Supreme Being (607 reputation)Supreme Being (607 reputation)Supreme Being (607 reputation)Supreme Being (607 reputation)Supreme Being (607 reputation)Supreme Being (607 reputation)Supreme Being (607 reputation)
Group: Forum Members
Posts: 46, Visits: 384
Steve Broad - 12/21/2018 10:48:01 AM
Hanaldo - 12/20/2018 10:45:37 PM
Fair enough, I hadn't checked the sizes. I tend to only use M6 and M10. 

And £1.86 each isnt THAT bad for small quantities!

I think that their prices have dropped so, I agree, that this isn't too bad for small numbers. However, I tend to buy in bulk and paid just under a £1 each for mine (similar size).


No the price is fine for me, but I do not want to pay 15 Pounds for delivery when I only buy fasteners for 6 Pounds!

Steve Broad
Steve Broad
Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
SHaas - 12/21/2018 11:01:13 AM
Steve Broad - 12/21/2018 10:48:01 AM
Hanaldo - 12/20/2018 10:45:37 PM
Fair enough, I hadn't checked the sizes. I tend to only use M6 and M10. 

And £1.86 each isnt THAT bad for small quantities!

I think that their prices have dropped so, I agree, that this isn't too bad for small numbers. However, I tend to buy in bulk and paid just under a £1 each for mine (similar size).


No the price is fine for me, but I do not want to pay 15 Pounds for delivery when I only buy fasteners for 6 Pounds!

Did you try

 https://shop.kvt-fastening.de/en/itemgroup/2001.html

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search