As resin systems go, GlassCast when fully cured is pretty scratch resistant. It can take a week or more for the resin to fully harden after its initial cure. Also be extra careful on weighing and mixing properly as a slight error could leave the resin softer than usual.
Scratches in GlassCast 3 normally can be polished or worst case sanded out.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|