Making a car door after the manufacturing the body


Author
Message
Zeyad Gamal
Z
Supreme Being (148 reputation)Supreme Being (148 reputation)Supreme Being (148 reputation)Supreme Being (148 reputation)Supreme Being (148 reputation)Supreme Being (148 reputation)Supreme Being (148 reputation)Supreme Being (148 reputation)Supreme Being (148 reputation)
Group: Forum Members
Posts: 17, Visits: 118
Hi guys, 

We are participating in the shell Eco marathon competition where we manufacture fuel efficient cars.

Due to rule changes for the 2019 season, we are now required to have a door on each side of the car. So we are now required to make a door on the other side of our current vehicle.

I was wondering if anyone has any suggestion on how we can cut the shape of the door and then put the part we cut back in its place and add a hinge to it ?

The main issue is that if we cut the door we will have a tiny gap when we put it back again, anyone got any idea how we can fix that ?

The body is made from carbon fiber and epoxy resin, manufactured by resin infusion technique.



Replies
Steve Broad
Steve Broad
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
Looking at the fit of the windscreen and light covers, the gap caused by a thin saw cut will be small in comparison :-)

However, if you plan to improve the fit of these items to improve the aerodynamics, then you may need to do something to help the air past the door gaps. One option would be to glue a small strip along the rear edge of the door, overlapping the gap.

With regard the the front edge of the door, perhaps a rubber strip would work?

This may or may not help, depending on whether any aerodynamic gain is offset by the increased weight. The air that will be affected is the boundary layer, which isn't moving relative to the car so I am not sure whether small door gaps will have any affect on aero efficiency.



Edited 7 Years Ago by Steve Broad
Furrari
F
Supreme Being (494 reputation)Supreme Being (494 reputation)Supreme Being (494 reputation)Supreme Being (494 reputation)Supreme Being (494 reputation)Supreme Being (494 reputation)Supreme Being (494 reputation)Supreme Being (494 reputation)Supreme Being (494 reputation)
Group: Awaiting Activation
Posts: 63, Visits: 99
Hi. Looking at the overall car I think the small gap around any doors you add will be very small in comparison to other problem areas. If you are realy bothered about this, do the regs allow tape over the joints.

In my opinion the biggest Aero problem is the drag imposed by the large amount of clearance around the wheels, particularly the back. These areas need to be drastically tightened up with the wheels filling the wheel apperture. Further improvements in this area would be to add covers to both the inside and outside of the wheels.

The aero of the edges of the windscreen area could also be improved by adding a big a radius to the outside corners to promote a better boundary layer. This could further improved by adding a curved blade or vane, about 2” clear of the corner and slightly forwards to guide the air coming off the screen down the side of the car.

A small splitter on the front would also help by raising the pressure centre at the front, channelling the air over the top of the car rather than underneath. This splitter would ideally need to be 3/4” clear of the ground but I don’t know if conditions will allow this.

I can’t tell from the pics, but is the floor a continuous, flat surface as it needs to be as each change of surface will cause drag. A diffuser would also help as it would reduce/fill the vacuum left by the car behind it.

All this lot is easy to say but not so easy to do. Keep up the good work.

M
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Zeyad Gamal - 7 Years Ago
Steve Broad - 7 Years Ago
Furrari - 7 Years Ago
Warren (Staff) - 7 Years Ago
Furrari - 6 Years Ago
Zeyad Gamal - 6 Years Ago
Steve Broad - 6 Years Ago
Zeyad Gamal - 6 Years Ago
Steve Broad - 6 Years Ago
Zeyad Gamal - 6 Years Ago
Steve Broad - 6 Years Ago
Zeyad Gamal - 6 Years Ago
Steve Broad - 6 Years Ago
Zeyad Gamal - 6 Years Ago
Steve Broad - 6 Years Ago
Zeyad Gamal - 6 Years Ago

Similar Topics