Hi!

I'm trying to laminate my first piece, and I'm having the some trouble every time I try to laminate it, lots of resin and bubbles at the edges.

I'm using the same process of this video: 
https://www.youtube.com/watch?v=IAdVO8Rkv6c
After all this process I use a peel ply a breather and a vacuum bag.

Someone can help me? Some pics below.



Hojo
Hojo
Supreme Being (289 reputation)Supreme Being (289 reputation)Supreme Being (289 reputation)Supreme Being (289 reputation)Supreme Being (289 reputation)Supreme Being (289 reputation)Supreme Being (289 reputation)Supreme Being (289 reputation)Supreme Being (289 reputation)
Group: Forum Members
Posts: 31, Visits: 957
jvmorais - 11/12/2018 5:20:04 PM
Hi!

I'm trying to laminate my first piece, and I'm having the some trouble every time I try to laminate it, lots of resin and bubbles at the edges.

I'm using the same process of this video: 
https://www.youtube.com/watch?v=IAdVO8Rkv6c
After all this process I use a peel ply a breather and a vacuum bag.

Someone can help me? Some pics below.



Corners will get bubbles if the fabric and/or bagging is bridging. Other than making sure during lamination fabric is conformed well, make sure to slowly/lightly apply vacuum and press in the corners with a rubber squeegee to ensure good consolidation in corners.