+x oekmont - 10/1/2018 7:14:07 AMRoom temperature cure doesn't mean wet layup. You could infuse the part as well. Using water isn't a good idea, as the water adds huge loads onto your mould, wich will likely deform it. A full vacuum bag, if done right, will not deform your mould.For such large pieces with large tolerances for the final shape, I would use styrofoam , than cover it with an glass cloth and epoxy and than smooth everything up with body filler.