Hi I'm looking for a dense foam which is lightweight which can be machined by hi speed turning which would accept a acrylic lacquer finish,I'm currently using a product called Rohacell but I'm looking for an alternative 
Replies
Ripple
Ripple
Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)
Group: Forum Members
Posts: 3, Visits: 14
Hi Matt , thanks for replying the foam I'm using at the moment is 71kg/m3 but looking for something a little harder say somewhere around 110kg/m3 .regards Richie
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (10K reputation)Composites Expert (Staff) (10K reputation)Composites Expert (Staff) (10K reputation)Composites Expert (Staff) (10K reputation)Composites Expert (Staff) (10K reputation)Composites Expert (Staff) (10K reputation)Composites Expert (Staff) (10K reputation)Composites Expert (Staff) (10K reputation)Composites Expert (Staff) (10K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Richie,

OK, well, our 80 would be the closest to what you have and it is a little denser than what you're using. After that we jump up to a 300 (unless you count our High Density Foam which is 90kg but doesn't have such a fine surface finish) so my suggestion would be to see how you get on with the 80.

All the best, Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search