XCR Black Epoxy Basecoat - Repelling from surface?


Author
Message
sjmn
s
Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)
Group: Forum Members
Posts: 4, Visits: 109
Hey folks,

I had a first attempt at carbon fibre skinning at the weekend and everything seems to have gone really smoothly apart from one issue.

We were skinning plastic parts, with a fairly rough surface to begin with, but still did a bit of a key with 120 grit sandpaper to be safe. I'm not sure exactly what type of plastic the parts were made from. At first, the basecoat went on really well but within a few seconds it started to split a bit, as if it was being repelled from the surface. For the majority of the part it didn't cause any problems but had prevented the carbon fibre from adhering properly to the part completely. The majority of the part is absolutely fine but there are little segments that didn't stick down as well. The fibre is being wrapped around the surface entirely, so I'm not worried about it delaminating and detaching completely, and the epoxy layers on top have applied really well. The issue came where the joins of the cloth didn't adhere well so it's not quite as neat as it could be. 

Unfortunately , we don't have much scope for using different types of parts - this is just a bit of fun, rather than for commercial sales or anything, but getting a perfectly finished part would be very satisfying. 

Is there any sort of primer or pre basecoat that we might be able to use that the basecoat could then adhere to?

Thanks!
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
It's simply a lack of adhesion. Plastic parts tend to be very low surface energy, which means they are difficult to bond to and you need to be extremely thorough with your prep work. It doesn't matter if the surface is textured, you need to do a thorough key all over with 60 or 80 grit. 120 grit is fine for most applications, but for plastic I would go rougher. Even doing an all over key with 60 grit and then deeply scoring the surface with a blade is a good idea.

You also want to make sure you degrease the surface extremely well before AND after you sand. Be careful using acetone for this, as if acetone effects the plastic then it will actually remove your key. Wax and grease remover is a more gentle solution.