The Rear Wing has finally gone from a concept to a finished part. Cosmetically it is far from perfect but it performs as per the the simulation model.

Carbon Copies Ltd
SebRS
SebRS
Supreme Being (245 reputation)Supreme Being (245 reputation)Supreme Being (245 reputation)Supreme Being (245 reputation)Supreme Being (245 reputation)Supreme Being (245 reputation)Supreme Being (245 reputation)Supreme Being (245 reputation)Supreme Being (245 reputation)
Group: Forum Members
Posts: 29, Visits: 558
Nice!

Don't forget my mail Wink

Regards,

Seb.
Joe
Joe
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 310, Visits: 1.5K
Awesome Wink

 



 


    A $1000 electronic device will always protect a 10 cents fuse
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Thank's for the comments fellas. This next one will be done using infusion so cosmetically should be better.

Carbon Copies Ltd
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
Top job!  Looks a very mild profile, are you using a profile modelling software package?  I reckon a clearcoat, flat and polish would have that looking perfect.  (I'm not a fan of infusion)
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Hi FLD, thanks for the comments. Yes the Profile was developed some years ago using CFD Software when I worked in the Aerospace Industry. I ran an Ally version on a Race Car back then and it worked well at a 7 Degree angle. This one is going on a Bikesport Race Car soon for testing/evaluation.

Regards Warren

Carbon Copies Ltd
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
I'd be interested in the results from that.  Are you using a piezo balance under the struts to measure downforce?
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
This is what I made.  It seems to have a bit more of a curve to the profile but it was just ripped off an existing known profile so nothing as exciting as CFD modelling.  The struts also look a bit lower tech than yours!


wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Nice work.
My limited experience shows that a "curved" trailing edge has a negative effect on the down force that the wing creates. The wing becomes a "spoiler" rather than a "wing" For it to be an effective wing it would need to be above the roof line. 

Carbon Copies Ltd
Edited 13 Years Ago by wozza
Leon
Leon
Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)
Group: Forum Members
Posts: 59, Visits: 606
Hii Wozzaa,

Have you ever work at Indonesia?? lipo cikerang, bekasi? Your work is great, I loved the CF  appearance.. is that hand-lay up? 

Regards

Leon
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search