Actually, the Composites Shrink Tape has no tack at all; you can only really use it in a wrapping operation (like around the outside of a pole etc.) and so if you're hoping to use it in the way we use the Release Breaker Tape in the new (sneak preview) video then it won't work.
Release Breaker Tape is really useful stuff and we'll be getting it in stock in the next 3-4 weeks (we have a shipment on order). Although it's not as good, brown parcel tape, because it's polypropylene, can perform a similar function if you're stuck for something to use for some of the applications you would use breaker tape for.
Best regards, Matt
Matt Statham Easy Composites / Carbon Mods - Technical Sales
|