I'm using XCR coating resin since last year. And never had difficulties to sand it dry. If it was hardened for at least two days, dry sanding always went smooth. But I've experienced the opposite this Summer. When it was impossible to dry sand resin that was hardened for 4-5 days. It clogs sandpaper or Abranet immediately. Also noticed weaker adhesion properties of that resin, no matter that previous coat was sanded with 220 paper. I have suspicion that it has a lot to do with air humidity. But maybe there are some additives available that would help to avoid such problems ?
Attachments
DSC_0580.JPG (577 views, 334.00 KB)
DSC_0583.JPG (532 views, 87.00 KB)
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
A light tack would suggest that the resin hasn't fully cured properly for some reason, be it a mixing or measuring issue or some kind of contaminant inhibiiing the cure.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
ZABAS - 7 Years Ago
Warren (Staff) - 7 Years Ago
ZABAS - 7 Years Ago
Warren (Staff) - 7 Years Ago
ZABAS - 7 Years Ago
Warren (Staff) - 7 Years Ago
ZABAS - 7 Years Ago
ZABAS - 7 Years Ago
Warren (Staff) - 7 Years Ago
ZABAS - 7 Years Ago
Warren (Staff) - 7 Years Ago
ZABAS - 7 Years Ago
Warren (Staff) - 7 Years Ago
ZABAS - 7 Years Ago
Warren (Staff) - 7 Years Ago
ZABAS - 7 Years Ago
Warren (Staff) - 7 Years Ago
ZABAS - 7 Years Ago
ZABAS - 7 Years Ago
ZABAS - 7 Years Ago
oekmont - 7 Years Ago
Hanaldo - 7 Years Ago
ZABAS - 7 Years Ago
oekmont - 7 Years Ago
ZABAS - 7 Years Ago
Hanaldo - 7 Years Ago
oekmont - 7 Years Ago
Matt (Staff) - 7 Years Ago
ZABAS - 7 Years Ago
Matt (Staff) - 7 Years Ago
ZABAS - 7 Years Ago
oekmont - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search