I already posted about my carbon fiber helicopter boom, for that I decided I'll bite the bullet and do alloy molds. 
I also need a carbon fiber helicopter canopy. Similar shape to a football but a bit bigger and open at the back, I'll attach a pic of one. It will have pretty thin wall thickness, generally they are about a half mm, maybe .6 or .7. So only a couple layers of weave. 
I will be making my own design on fusion 360 and milling the plug on my cnc. The process that makes the most sense to me is milling each plug half (mold will be split down the middle lengthwise, right and left half) out of mdf or foam, spraying it with layers of duratec primer, sand and polish, then attach each plug half to a flat sheet of melamine or some other rigid plastic to create base for mold flanges and proceed to make fiberglass mold halves from that. I would prefer to skip the plug stage and go straight to milling the molds, but it just doesn't seem to work out as well as making fiberglass molds from a plug.  From the female molds I will vacuum bag a carbon fiber wet lay up. 
does this sound like a good plan or is there an easier/better way considering I have a cnc? Another variation would be attaching the 2 plug halves together to make a complete plug before applying duratec,  then split into 2 molds using the method shown in the air box video, but i feel that it will be less work to just attach the 2 halves to flat sheets for making the molds, just need to make sure both sheets are perfectly flat planes. 

Reply
quinn
q
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 155, Visits: 992

clear coat added 6 grams, not bad. All in all I would say it came out pretty decent. Definately rushed with the clear coat on this one. I'll consider this the practice canopy. I ordered some chemical release for the next one so i don't have to deal with the nightmare of tacking fabric down to pva, also should be able to avoid clear coat next time. Also I used web lock weave for this one which made fraying more controllable but I think it really hindered the drapability of it around compound curves which meant I needed to cut it in a few places to get it to lay down. Ordered non web lock for the next one. 
Thanks everyone for all the advice and help. I'm pleased with the results and the next one will be better. I definately won't be buying anymore helicopter canopies. Infused carbon is the way to go. 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
Warren (Staff) - 7 Years Ago
quinn - 7 Years Ago
Warren (Staff) - 7 Years Ago
Hanaldo - 7 Years Ago
SleepingAwake - 7 Years Ago
quinn - 7 Years Ago
quinn - 7 Years Ago
SleepingAwake - 7 Years Ago
oekmont - 7 Years Ago
quinn - 7 Years Ago
oekmont - 7 Years Ago
Steve Broad - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
oekmont - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
Steve Broad - 7 Years Ago
quinn - 7 Years Ago
SleepingAwake - 7 Years Ago
oekmont - 7 Years Ago
quinn - 7 Years Ago
SleepingAwake - 7 Years Ago
quinn - 7 Years Ago
                     EasyComposites offers Easy-Lease at £6.80 for 100ml
Steve Broad - 7 Years Ago
quinn - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
Steve Broad - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
SleepingAwake - 7 Years Ago
quinn - 7 Years Ago
quinn - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
oekmont - 7 Years Ago
quinn - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
quinn - 7 Years Ago
oekmont - 7 Years Ago
quinn - 7 Years Ago
quinn - 7 Years Ago
Warren (Staff) - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search