I already posted about my carbon fiber helicopter boom, for that I decided I'll bite the bullet and do alloy molds. 
I also need a carbon fiber helicopter canopy. Similar shape to a football but a bit bigger and open at the back, I'll attach a pic of one. It will have pretty thin wall thickness, generally they are about a half mm, maybe .6 or .7. So only a couple layers of weave. 
I will be making my own design on fusion 360 and milling the plug on my cnc. The process that makes the most sense to me is milling each plug half (mold will be split down the middle lengthwise, right and left half) out of mdf or foam, spraying it with layers of duratec primer, sand and polish, then attach each plug half to a flat sheet of melamine or some other rigid plastic to create base for mold flanges and proceed to make fiberglass mold halves from that. I would prefer to skip the plug stage and go straight to milling the molds, but it just doesn't seem to work out as well as making fiberglass molds from a plug.  From the female molds I will vacuum bag a carbon fiber wet lay up. 
does this sound like a good plan or is there an easier/better way considering I have a cnc? Another variation would be attaching the 2 plug halves together to make a complete plug before applying duratec,  then split into 2 molds using the method shown in the air box video, but i feel that it will be less work to just attach the 2 halves to flat sheets for making the molds, just need to make sure both sheets are perfectly flat planes. 

Reply
Lester Populaire
L
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
Hanaldo - 8/12/2018 2:40:40 AM
Dont worry about the gauge, they are all going to be inaccurate in one way or another. Some may be better calibrated than others, but at the end of the day the number they point to really doesn't matter. Keep in mind that elevation above sea level and atmospheric conditions will change the reading the gauge gives you as well. So one day it might read 26", the next day it could be 30mm past the 30" mark - and I promise you wont be pulling 32" of vacuum! 

Stick with what you've got. Your pump should be perfectly capable of pulling full vacuum, so if it goes quiet and stops emitting oil vapour when the gauge says you are at full vacuum then you are likely at full vacuum. If you're really worried about it, do some playing around and infuse some flat sheet. You'll learn a lot, and you'll also be able to look at the flat sheet and diagnose any problems - pump related problems are going to be obvious.

I would highly recommend infusing some flat sheets of glass fiber and carbon fiber and whatever to figure out all small details of the process!

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
Warren (Staff) - 7 Years Ago
quinn - 7 Years Ago
Warren (Staff) - 7 Years Ago
Hanaldo - 7 Years Ago
SleepingAwake - 7 Years Ago
quinn - 7 Years Ago
quinn - 7 Years Ago
SleepingAwake - 7 Years Ago
oekmont - 7 Years Ago
quinn - 7 Years Ago
oekmont - 7 Years Ago
Steve Broad - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
oekmont - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
Steve Broad - 7 Years Ago
quinn - 7 Years Ago
SleepingAwake - 7 Years Ago
oekmont - 7 Years Ago
quinn - 7 Years Ago
SleepingAwake - 7 Years Ago
quinn - 7 Years Ago
                     EasyComposites offers Easy-Lease at £6.80 for 100ml
Steve Broad - 7 Years Ago
quinn - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
Steve Broad - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
SleepingAwake - 7 Years Ago
quinn - 7 Years Ago
quinn - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
oekmont - 7 Years Ago
quinn - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
quinn - 7 Years Ago
oekmont - 7 Years Ago
quinn - 7 Years Ago
quinn - 7 Years Ago
Warren (Staff) - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search