Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
I would suspect if you slow the infusion down a bit, you will give more time for the resin to soak through and all should be fine. However you never know until you try it.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|