i have experience by 2 sides mold by presing each other and trust me part comes very hard but problem is that air not go out and part is bad cometic look also some places change color. from 10 parts good been with straight pattern and around to good look like 2 not more, so i suggest vacuuming or infusion or do pre preg with autoclave self made.
|