			            Hello guys
  i done a lot wrappings in carbon with epoxy and polyster resins what is the question- polyster resin is bad that after some time laquer start to go low in surface and you have to ressand as polyster resin flexible and always moving. i tryed epoxy i liked it a lot. But i do not understand before some years i got from china parts in carbon wrapped it look like epoxy was only polished for hard surface after wrap or i mistaken? also companies in malaysia that has very good names in wrapping stuff in carbon give like 2 years that you not scratch parts maybe anyone know how that can be? what they use? any clue? im attaching their work of ebrake handle. what you think resin can be used i know that is hard to gues.
  Also how they can wrap even bmw grills with blades for me its like space or mercedes grill logo im attaching images as i know that carbon can be connected nicely but from images i think they done from 1 pieces.
 
  one more thing im searching for pump and everything to start infusion is it hard? as what i saw you getting part perfect finish so you can put on a car and drive.
 
  Thank you a lot guys for help and sorry from my english im east from europe                
			            				
			                                 
                     
                                            
                         
                    
                  
             |