Hello there,
I'm just starting out making bass guitars using carbon fibre (wet lay vacuum bagging wrapping a core material) It'll be great use joining you guys on the forum and i look forward to learning more on composite engineering.
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Welcome to the Forum!  We have a wealth of information here which should help you.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
K_J
K
K_J
posted 7 Years Ago HOT
Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)
Group: Forum Members
Posts: 2, Visits: 25
jebroad - 6/30/2018 9:16:59 PM
Hello there,
I'm just starting out making bass guitars using carbon fibre (wet lay vacuum bagging wrapping a core material) It'll be great use joining you guys on the forum and i look forward to learning more on composite engineering.

Hi, 

I've started a project for my apprenticeship which is making a carbon fibre bass guitar. Do you have any knowledge on how I can do this as I have never worked with Carbon Fibre moulding before. 