I agree with hanaldo, that internal bladder moulding would be the optimal route to go.
However I think those are made positive over a core. First the tube diameter gets bigger towards the knots. And from the pictures it looks like it does so in quite an irregular way. Would be strange for negative moulding. Secondly the surface doesn't seem perfectly flat. Just a slight waveiness. Last, but not least, the surface is made with a carbon sleeve. It is really difficult to get an even weaving texture with a sleeve while using internal bladder moulding. In this case I would tend to say it's impossible. At least at the orthogonal end plugs. Quite a craftsman, to get such a nice finish with positive methods. This needs practice.
|