Hello All. I'm looking for whatever info, advice or even just comments I can get on creating a laminated composite timber beam.
It's part of a student project comparing the structural properties of timber vs. laminated timber vs. laminated composite/timber 
The test beams are 1/4 scale so approx. 40mmx90mm and a metre long.

It would be simple enough to incorporate a single piece of pultruded CF but I'd like to try layers of cloth between each of the 10 timber lamellas.

Any suggestions on the composite material and resins or adhesives much appreciated!

Many thanks



Replies
oekmont
oekmont
Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
Regular cloth doesn't make that much sense, as 50% of the fibres are basically wasted. Also, layering the cloth between each layer of timber isn't optimal, as the inner layers take much less load, reducing both stiffness and strength compared to the same material placed outside.
Regular epoxy laminating resin and unidirectional carbon or (!) glass should work fine. Ideal would be either a vacuum or regular veneer press

21TonyK
2
Forum Member (37 reputation)Forum Member (37 reputation)Forum Member (37 reputation)Forum Member (37 reputation)Forum Member (37 reputation)Forum Member (37 reputation)Forum Member (37 reputation)Forum Member (37 reputation)Forum Member (37 reputation)
Group: Forum Members
Posts: 4, Visits: 25
oekmont - 5/27/2018 5:52:04 PM
Regular cloth doesn't make that much sense, as 50% of the fibres are basically wasted. Also, layering the cloth between each layer of timber isn't optimal, as the inner layers take much less load, reducing both stiffness and strength compared to the same material placed outside.
Regular epoxy laminating resin and unidirectional carbon or (!) glass should work fine. Ideal would be either a vacuum or regular veneer press


Many thanks. I like the idea of laminating it all myself but can see the logic of just one layer. I have looked at a lot of published research online but really like the decorative finish of carbon and timber (architecture student)