Hi,  l'm looking for a suitable means to make a 90 degree bend in 40mm dia woven tube.
Default, messy idea is to use an abs plastic elbow and wrap with carbon fibre tape and resin.  Would that work...  or is there a 'stock'  carbon item that would be reasonable?
Suggestions welcome!

Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Could you mitre the join and bond the tubes together with a 5 minute epoxy (or something more structural if needed, but you'd need to make a jig to hold the tubes together while it cured), then wrap with carbon to reinforce? 
Mutineer
M
Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)
Group: Forum Members
Posts: 3, Visits: 8
Hanaldo - 5/26/2018 1:59:31 AM
Could you mitre the join and bond the tubes together with a 5 minute epoxy (or something more structural if needed, but you'd need to make a jig to hold the tubes together while it cured), then wrap with carbon to reinforce? 

Thanks, yes, that's another option, especially if plugged internally and also reinforced externally with an alloy jig, which I think would need to be permanent.  Otherwise I think I would need a couple of 45 degree mitres to avoid a sharp corner and that these would need both internal and external reinforcement.  I thought an ABS fitting could act as a former, with fewer point loadings than a mitre, and provide the inner layer of a sandwich, but I was wondering if anyone had tried that.