Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
Ideally you want a proper built vessel or at least something that has been tested to take the required pressures and levels of vacuum without failure.
You can make a throw away catch pot/bag by making a small bag in vacuum bagging film and filling it with 3 or 4 layers of breather cloth. Insert it between the pump and bag and the breather will catch and soak up any resin that comes through. It is , however, ruined after each use as the resin goes off, but can be a good temporary solution.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|