Aluminium Honeycomb thinner than 10 mm - ideas how to machine it thinner?


Aluminium Honeycomb thinner than 10 mm - ideas how to machine it thinner?
Author
Message
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
Hi,

I have just ordered a piece of the smallest cell honeycomb, but for one of my projects I would really like to have the material as this as 4 - 5 mm ..

Do you have any suggestions as to how I might machine it thinner?

I was considering cutting out a small section of the un-expanded stock, and then making a jig to told the piece compressed, while milling it thinner on my mill.

Does that sound like a feasible method?

Also, do you have any experience with how titanium bonds to (and into) Epoxy based composites, are you aware of any "pitfalls" with this metal?

I have successfully bonded aluminium before, using West Systems Resins, and Ti should be similar, but I'm wondering about your High Temp resin?

Cheers

Dravis

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
You might want to PM Dravis as i doubt he would regularly look back in this forum section without prompting.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant