	Group: Forum Members 	        
    Posts: 592, 
    Visits: 1.9K 
    
 
          
		     | 
				                       
                 
                
                    
			            Hi,
  I have been doing some testing on the Alu honeycomb -- 
  Results so far:
  I have successfully cut smaller un-expanded pieces of the small cell honeycomb into two layers 4 mm in thickness, by using an ordinary fine toothed hacksaw .. I simply clamp a short piece in my vice (in the direction of expansion) and allow about 5 mm to stick out, then cut this lenght, and move the piece up another 5 mm, and so on.. as soon as about 5 mm i free above the hacksaw blade, I put a small c-clamp on above the hacksaw blade.
  This produces two pieces of thinner honeycomb, but with an uneven, rough finish on one side... i then clamp the piece flat in the vice and simply sand it nice and flat on the rough hacksaw cut side..
  For precision parts I use my milling machine, to ensure perfectly even thickness.
  A 4 mm test piece bonded between two layers of 3x 200 g carbon supported a weight of more than 60 kg per square cm, with no deformation
  Permanent deformation did not occur until the load surface was reduced to less than 1 square cm with 70+ kg on one point. 
  The 6 cm long piece did not crack or deform permanently when clamped by 1 cm at one side and loaded with 70 kg+ clamped to 1 cm on the other end.                
			            
  				
			            "Sapere Aude"... Dare to KNOW!
  The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...
  103% of all people do not understand statistics...
  Do not adjust our mind, theres a fault in reality :-)                     
                     
                                            
                         
                    
                  
             |