Group: Forum Members
Posts: 9,
Visits: 48
|
I am vacuum bagging the hull of a boat and the sealing tape isn't sticking well to the fibreglass. The fibreglass was laid 7 days ago. I have tried washing thoroughly with acetone and also a light sand, but tape is still not creating a good seal. Any suggestions? Does the fibreglass need to cure longer? Any assistance would be appreciated.
|