posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 13,
Visits: 27
Once the putty is hardened, can you add more or will the bond not be strong enough?
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Epoxy putty
sebgron
-
13 Years Ago
New putty won't stick properly to hard putty so what I would suggest if you want to add more putty...
Matt (Staff)
-
13 Years Ago
Makes sense. Thanks!
sebgron
-
13 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search