I'm new here. Hello everyone! I'm interested in working with someone to design and make custom musical instrument cases, beginning with saxophones. Is there anyone in the USA who does something like this already? 

Thanks! 
Reply
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
I have made several instrument cases, along with a number of gun-cases and boxes for sensitive equipment.

I normally just make a plug the  size and shape of the outside of the box I want, then make a mould (usually 2 or 3 part mould)

I use a commercial company that waterjet cuts the foam for the internals, they can cut any shape from 3D files

My usual layup is 2 inside layers of  kevlar/carbon mix and one outside of pure carbon, some customers liked the kvelar mix on the outside as well, so those were made with a "kevlar-carbon-kevlar" layup

The really big cases were made with 4 layers in various mixes of layers two of my own cases have hinges made from EC flexible Epoxy and pure Kevlar weave - 

I have used both infusion and vacuum bagged wet-lay for the boxes 


"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search