Reproduction from pattern without damaging original


Author
Message
James Buckle
James Buckle
Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)
Group: Forum Members
Posts: 1, Visits: 3
I'm trying to take a copy of a plastic part I have which is slightly the wrong shape/angle - my plan being to modify the original, then create a better version while keeping the old one as a backup for when I mess it up!

The original has a textured surface (your standard grippy plastic surface 0.5mm patterning). I'd like to temporarily and non-destructively fill that, so I can take a multi-part mould from it. I'm obviously concerned about releasing the pattern from the mould afterward - what technique would you use?
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Better to just take a quick splash mould of it as is, then use that mould to produce a fibreglass copy that you can modify and paint and bring up to the finish you want.

The splash mould can just be 3-4 layers of csm and regular polyester or vinyl ester laminating resin, as cheap as you like. 