Composite panel construction *need advice*


Author
Message
gully
g
Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)
Group: Forum Members
Posts: 2, Visits: 104
Hi I need advice. I am going to build a camper using composite panels. The panels will be constructed using a 2inch foam core (XPS) with 1.8mm GRP fiberglass skins on each side. The fiberglass skin is a laminate that is manufactured and then shipped to me. So its not a wet layup, I think thats what its called. Sorry am new to all this. The skin or sheeting comes in a large roll, its gel coated (on only one side I believe)

I am considering an Adtech epoxy product to adhere the sheeting to the XPS foam sheet. Do you think with this type of layup, using a laminate sheet, instead of using fiberglass cloth and resin (wet layup), should I vacuum bag these panels? Will it give me the best lamination? Could i just use bricks or some kind of weight on top of the panel and get just as good results? I don't know much about vac bagging. I would have to buy the supplies and work it out. If anyone has experience with this, or if you know of some other threads or forums. I need any help I can get to feel confident that my panels will hold and not delaminate on me. 

Also, I have read about various procedures to scuff up the foam to get better adhesion. Any thoughts? 


Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
I see no reason why you can't do both at once with that method.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant