Hi all,

I'm just starting down the route of building a large oven for use of prepregs etc but for the time being I need to epoxy wet lay projects such as this and for that matter I'm not sure I would even be able to get hold of a low temp cure prepreg from the materials I need to use.

The project is small sidecar fairing much like an F2 Racing Sidecar only a kart sized one that is raced on kart tracks. Its about 1.5m long and has a fair amount of shape. Top end speeds are 60-70mph on larger kart circuits. There tends to be a some body contact and your average polyester/gelcoat fairing tends to look crap after only a few meetings due to the cracking nature of the gelcoat as the bodywork flexes and takes knocks from the other tricycle bumper cars! 

The bodywork needs to have some flex and 'give' at the extremities whilst being fairly sturdy around the middle part and mounting points. I guess the nearest other subject would be a white water racing kayak or similar. I will achieve this by use of multiple materials (Glass, Diolen, Carbon) where appropriate. I know I cant expect something that gets abused like this to look great forever or last forever but keeping it looking fresh for as long as possible would be preferable.

Sorry if that was all a bit long winded but once people have quizzed me about my intended use I would have ended up writing it all in the end anyway.

So...... I want a black surface finish, dont want to paint it and dont want carbon on the outer skin (looks great but is dangerous in a heavy accident). First thought it to use black Diolen for an all over first ply. I will never get this layup to stay down everywhere so will bag it, being a fairly big job I know that I'll end up with dry bits/air bubbles here and there no matter how careful I am partly due to not being able to get a coat of resin to stay on the released mould first. I have some GC50 epoxy compatible clear gelcoat but after doing some tests I'm sure it will de-laminate/crack after some impacts.

Next thoughts are to use fumed silica to spray some thickened resin onto the mould surface as a thin epoxy gelcoat which will most likely end up looking milky? Then I'm thinking maybe just add black pigment as well as the silica or will this go grey rather than black?

Any got any experience with this or have any thoughts or ideas how else I could achieve a decent looking but hardy  black surface on my mobile battering ram?



My mould and pattern






Edited 7 Years Ago by CaveDweller
Reply
CaveDweller
CaveDweller
Supreme Being (88 reputation)Supreme Being (88 reputation)Supreme Being (88 reputation)Supreme Being (88 reputation)Supreme Being (88 reputation)Supreme Being (88 reputation)Supreme Being (88 reputation)Supreme Being (88 reputation)Supreme Being (88 reputation)
Group: Forum Members
Posts: 10, Visits: 279
Thanks for the reply, I've just had a look at the Kraibon system and it looks very interesting, definitely something I will investigate in due course, thanks for the heads up Smile 

For now I will try and keep things simple as possible and stay monolithic. Being able to achieve a good surface finish without post layup dressing is the primary goal and playing with the varying needs of different areas of the fairing robustness (is that a word?) along the way. The Diolen seemed like a good cost effective alternative to Kevlar with its elongation and abrasion qualities, comes in Black too! There is also black Twaron I guess.

Carbon where the structure needs stiffness and linking up the mounting points thickening the laminate internally to  3mm or so.  Three or four plies of 200/300g diolen/glass/aramid in other areas....... still need to do a few more test pieces before deciding. I'm open to debate and trials.

Just wondered about the aspect of making an epoxy gel coat to be applied sparingly, how cloudy it gets with the silica  and if black pigment will just make it dark grey?. I want proper black or clear with black Diolen/Twaron showing through.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
CaveDweller - 7 Years Ago
scottracing - 7 Years Ago
CaveDweller - 7 Years Ago
M.R. - 7 Years Ago
Fasta - 7 Years Ago
CaveDweller - 7 Years Ago
CaveDweller - 7 Years Ago
Fasta - 7 Years Ago
CaveDweller - 7 Years Ago
M.R. - 7 Years Ago
CaveDweller - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search