Hello Easy Composites.
Due to some unforeseen circumstances I have had to delay my adventures in mould making. It's now three years since I purchased the Uni-Mould Complete Mould Making Kit. The resin containers have never been opened but will it still be usable if I were to use within the next six months? It has been stored in a garage out of the sunlight but otherwise subject to normal UK temperatures.

Thanks for your help
Ian




Marcos Mantula blog
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Open it and have a look. It will have seperated out, but if it hasnt gelled and you can mix it back together then it should still be ok.

It is very likely buggered though unfortunately, especially the vinyl ester components.