First time with Uni-Mould. I made enough resin to do only two layers of 450CSM, Mistake in calculation, for a hood that I am building. That same miscalculation meant that I did not have enough MEKP on hand to make enough for the final two layers. Can I come back and add the additional reinforcement a week later? Have to travel and ran out of time. This is not a production mould. I hope to get two good hoods out of it. 
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Yes you can.  All you will need to do is give the surface a good key with 120 grit sand paper and a clean  before coating again.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search